Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.411 MPa | 4410.8 psi | ASTM D638 |
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |