Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 297 MPa | 43100 psi | ASTM D-638 |
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Tensile Strength | 297 MPa | 43100 psi | ASTM D-638 |
PlastiComp Velocity® LCF40-PA66 High Flow Nylon 66, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Strength | 297 MPa | 43100 psi | ASTM D-638 |
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |