Tensile Strength 4.905 MPa
711.4 psi
ASTM D412
E-Polymers EFLEX® V2045 SEBS/TPV
V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq..