Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 4.14 MPa | >= 600 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 0862 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tensile Strength | 4.14 MPa | 600 psi | ASTM D412 |
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Tensile Strength | 4.14 MPa @Strain 100 % |
600 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.14 MPa @Strain 100 % |
600 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.14 MPa @Strain 100 % |
600 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.14 MPa | 600 psi | ASTM F152 |
Garlock GRAPH-LOCK® 3123/3125 Graphite Sheet Gasketing A pure graphite sheet. Thicknesses |
|||
Tensile Strength | 4.14 MPa | 600 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1113 P (SIS) Linear Block Copolymer Description: Kraton D1113 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra.. |
|||
Tensile Strength | >= 4.14 MPa | >= 600 psi | BAM 1211 |
Kraton® G4609 H (SEBS) with Oil Description: Kraton G4609 H is a white mineral oil extended linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. Nominal oil content of the polymer is .. |
|||
Tensile Strength | 4.14 MPa | 600 psi | ASTM D412 |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 4.14 MPa | 600 psi | ASTM D412 |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 4.14 MPa | 600 psi | |
Teknor Apex Elexar® EL 3954-50 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | >= 4.14 MPa | >= 600 psi | Compound Property |
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T.. |
|||
Tensile Strength | 4.14 MPa | 600 psi | Silicone Property; ASTM D412 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Tensile Strength | 4.14 MPa | 600 psi | |
AlphaGary AlphaSeal™ 388 D Polyolefin Thermoplastic Elastomer AlphaSeal™ 388 D is a polyolefin/TPE material recommended for a liner in wine bottle caps. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resistanc.. |