Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 39.1 MPa | >= 5680 psi | ASTM D 638 |
Karina 822-18/599-CRB-LMP Gray PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.1 MPa | >= 5680 psi | ASTM D 638 |
Karina E 822-10/148-CRB-LMP White PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.1 MPa | >= 5680 psi | ASTM D 638 |
Karina E 854-35/1-A-ERYB Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.1 MPa | >= 5680 psi | ASTM D 638 |
Karina E 854-35/1-Y-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.1 MPa | >= 5680 psi | ASTM D 638 |
Karina E 857-35/1-A-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |