Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.2 MPa | 3800 psi | ASTM D412 |
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Tensile Strength | 26.2 MPa | 3800 psi | ASTM D638 |
Ensinger Tecatron® XP-65 Compression Molded PPS Compound, 30% Fiberglass with 15% PTFE Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 26.2 MPa | 3800 psi | 2 in/min; ASTM D638 |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Tensile Strength | 26.2 MPa | 3800 psi | 2 in/min; ASTM D638 |
Braskem TI4015F2 Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the r.. |
|||
Tensile Strength | 26.2 MPa | 3800 psi | ASTM D638 |
Aaron Industries AAROPRENE® CFPP 2030 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |