Tensile Strength 2600 MPa
377000 psi
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber
Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance ..
Tensile Strength 2600 MPa
377000 psi
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (..