Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.250 MPa | 36.3 psi | ASTM D 412 |
Eurofoam Evacell EVA 30 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |