Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 35.5 MPa | 5150 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |