Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 240 MPa | 34800 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |