Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 33.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 33.00 MPa
4786 psi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar..
Copyright © lookpolymers.com All Rights Reserved