Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 22.6 MPa | 3280 psi | ASTM D638 |
Teknor Apex APEX® 4303 Polyvinyl Chloride Compound Notes: Clear; Flame Retardant ; Non-Tarnishing; SPT Insulation/Jacketing temperature Rating: 75°CInformation Provided by Teknor Apex |