Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 22.6 MPa | 3270 psi | ASTM D638 |
Samyang Trilen® 9550AC Polypropylene, General Purpose Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang. |