Polymer Property : Tensile Strength = 31000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 214 MPa
31000 psi
IPC 2.4.19
Rogers Corporation Ultralam® 3908 Liquid Crystalline Polymer Circuit Material
ULTRALAM® 3908 bondply is used as a bonding medium between copper and the dielectric material. This product was developed specifically for multi-layer substrate constructions. This adhesiveless f..