Mechanical Properties Metric English Comments
Tensile Strength 30.5 MPa
4420 psi
ASTM D412
GRECO ISOTHANE 1685AE Polyether TPU Resin
ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf..