Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.207 MPa | 30.0 psi | Typical; ASTM D3574-75 Test E |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Strength | >= 0.207 MPa | >= 30.0 psi | ASTM D3574-75 Test E |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation. |
|||
Tensile Strength | 0.207 MPa | 30.0 psi | |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |