Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.85 MPa | 558 psi | Fluorosilicone Property; ASTM D412 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Tensile Strength | 3.85 MPa | 558 psi | Fluorosilicone Property; ASTM D412 |
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Tensile Strength | 3.85 MPa | 558 psi | Silicone Property; ASTM D412 |
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used .. |