Polymer Property : Tensile Strength = 3.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 3.20 - 9.00 MPa
464 - 1310 psi
ASTM D 638
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..