Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 201 MPa
29200 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Tensile Strength 201 MPa
29200 psi
ASTM D638
Kolon KOPA® KN333C22 CF Reinforced Nylon 66
Carbon 22%, high strengthApplications Cylinder piston partsInformation provided by API-Kolon.
Tensile Strength 201 MPa
29200 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..