Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 29.4 MPa | >= 4270 psi | ASTM D 638 |
Karina 837-35/1-E-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8210F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8521H TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8800F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8910K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8915K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A8970A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A9511U Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® D6820 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® D7220 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | >= 29.4 MPa | >= 4270 psi | ASTM D 638 |
Karina 802-18/462-C-ERB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 29.4 MPa | 4270 psi | |
Taiwan Sheen Soon Sheenthane® A9830 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |