Tensile Strength 196.2 MPa
28460 psi
ASTM D638
E-Polymers SEPAZ® V235A 35% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..