Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 18.7 MPa | 2710 psi | Optimum; With provided formulation; ASTM D638 |
PolyOne Geon™ Specialty Suspension Atlas E 43 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 43 is a non-chain modified ultra-high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical properties, fo.. |