Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 185 MPa | 26800 psi | ASTM D638 |
Kuraray Genestarâ„¢ GN2330 Nylon, 33% Glass Filled Standard V-0 Grade. Features a balance of mechanical strength, mold-ability, and dimensional stability. Well suited for a wide range of electrical and electronic components. |
|||
Tensile Strength | 185 MPa | 26800 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |