Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 181 MPa | 26300 psi | ASTM D-638 |
PlastiComp Complet® LGF40-PEI Polyetherimide, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long glass fiber reinforcementInformation provided by PlastiCo.. |
|||
Tensile Strength | 181 MPa | 26300 psi | ASTM D638 |
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66 High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon. |
|||
Tensile Strength | 181 MPa | 26300 psi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Tensile Strength | 181 MPa | 26300 psi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |