Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.6 MPa | 3860 psi | ASTM D638 |
Aaron Industries AAROPRENE® TFIPP 2040 High Impact Talc Filled Polypropylene AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |