Polymer Property : Tensile Strength = 2593 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 17.88 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2593 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
S&E Specialty Polymers GA-1057H1-VW1LF PVC
Application: Lead free 105° C, flat ribbon cable insulation.Information provided by S&E Specialty Polymers