Tensile Strength 17.9 MPa
2590 psi
Average; ASTM D412 Method A
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.