Polymer Property : Tensile Strength = 25600 psi
Polymer Property :
Tensile Strength =
25600 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength
177
MPa
25600
psi
50 mm/min; ISO 527
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.