Polymer Property : Tensile Strength = 23600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 163 MPa
23600 psi
50 mm/min; ISO 527
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 163 MPa
23600 psi
50 mm/min; ISO 527
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.