Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1620 MPa | 235000 psi | 48 HRC |
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |