Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1610 MPa | 234000 psi | 48 HRC |
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |