Polymer Property : Tensile Strength = 2290 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 15.8 MPa
2290 psi
ASTM D638
Teknor Apex APEX® 4150 Polyvinyl Chloride Compound
Notes: Sunlight Resistant; 60°C Oil Resistant; Ultra Low Temperature Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex