Tensile Strength 1.50 MPa
218 psi
ASTM D412
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc..
Tensile Strength 1.50 MPa
218 psi
Shin-Etsu Silicones KE-3493 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 1.50 MPa

@Strain 20.0 %
218 psi

@Strain 20.0 %
ISO 37
BASF Elastollan C 65 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tensile Strength 1.50 MPa
218 psi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Tensile Strength >= 1.50 MPa
>= 218 psi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Tensile Strength 1.50 MPa

@Strain 20.0 %
218 psi

@Strain 20.0 %
ISO 37
BASF Elastollan C 70 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tensile Strength 1.50 MPa
218 psi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..