Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 148 MPa | 21500 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Tensile Strength | 148 MPa @Treatment Temp. 1090 °C |
21500 psi @Treatment Temp. 1990 °F |
|
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |