Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 14.756 MPa @Temperature 136 °C, Time 605000 sec |
2140.2 psi @Temperature 277 °F, Time 168 hour |
Aged |
S&E Specialty Polymers TufFlex™ GTPE-2272 TPE Compound Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers |