Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 14.22 MPa | 2063 psi | ASTM D412 |
E-Polymers EFLEX® S2070 Transparent S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |