Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1410 MPa | 204000 psi | 44 HRC |
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |