Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.4 MPa | 1950 psi | |
AlphaGary Garaflex™ E X 00-207F UV-FG LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated flame retardant, flexible jacket compound with sunlight & fungus resistant properties |