Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 195 MPa @Temperature 23.0 °C |
28300 psi @Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 195 MPa | 28300 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Tensile Strength | 195 MPa | 28300 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Tensile Strength | 195 MPa | 28300 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |
|||
Tensile Strength | 195 MPa | 28300 psi | ASTM D638 |
DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET) 36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performan.. |
|||
Tensile Strength | 195 MPa | 28300 psi | ASTM D638 |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |