Tensile Strength 19.032 MPa

@Temperature 100 °C,
Time 864000 sec
2760.4 psi

@Temperature 212 °F,
Time 240 hour
Aged
S&E Specialty Polymers TufTech™ GA-7056-1002 PVC Compound
Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers