Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 1870.4 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.896 MPa

@Time 605000 sec
1870.4 psi

@Time 168 hour
Aged in ASTM Oil #2
S&E Specialty Polymers TufFlex™ GA-1042FR-60-0-405 Black TPE Compound
Application: An oil resistant, flexible, 60°C rated jacketing compound.Information provided by S&E Specialty Polymers