Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 12.8 MPa @Strain 100 % |
1860 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JA612EA Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 12.8 MPa | 1860 psi | ASTM D412 |
S&E Specialty Polymers GA-2285FR PVC Application: 80°C clear flame retardant PVC compound.Information provided by S&E Specialty Polymers |