Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1255 - 1315 MPa | 182000 - 190700 psi | |
Plansee DENAL® 917 108 XXX (1) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Tensile Strength | 1250 MPa | 182000 psi | 40 HRC |