Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 18.079 MPa @Temperature 136 °C, Time 605000 sec |
2622.1 psi @Temperature 277 °F, Time 168 hour |
Air Oven Aging |
S&E Specialty Polymers TufFlex™ GA-509-80-5 TPE Compound Application: A Matte Finish, Flexible, Sunlight Resistant, 105?C Jacketing Compound with 60?C Oil Resistance.Information provided by S&E Specialty Polymers |