Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 17.4 MPa @Strain 100 % |
2520 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5D05 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound, designed primarily for extruded sheet and tile applications.Information provided by PolyOne |
|||
Tensile Strength | 17.4 MPa | 2530 psi | ASTM D638 |
Teknor Apex APEX® 84132UV Polyvinyl Chloride Compound Notes: Sunlight Resistant Tray Cable Coax Jacket Temperature Rating: 80°CInformation Provided by Teknor Apex |