Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 17.24 MPa | 2500 psi | ASTM D412 |
Kraton® G2874 GO-N (SEBS) Compound Description: Kraton G2874 GO-N is a compound supplied from North America in the physical form identified: Kraton G2874 GO-N - supplied as a dusted, dense pelletRegion: North AmericaApplications: Com.. |