Polymer Property : Tensile Strength = 165 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 1.14 MPa
165 psi
ASTM D412
Parker Chomerics CHOFORM® 5560 Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..