Mechanical Properties Metric English Comments
Tensile Strength 111.8 MPa
16220 psi
ASTM D638
E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..