Mechanical Properties Metric English Comments
Tensile Strength 112 MPa
16200 psi
ASTM D638
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..