Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 111 MPa | 16100 psi | ASTM D882 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |